By consideration of kinetic features of thermal degradation of polybutadiene in a gaseous fluid of air, an argon and a carbon dioxide it is erected that increase of temperatures augments velocity of process of the cyclization of rubber, leading to formation of carbon. Indispensable and sufficient stay time of a fragment of rubber in reactionary environment compounds 20 minutes. Recommended temperature range of waste-handling lies within 500-600°С. In a kind of complication of process of thermal degradation of polybutadiene studies of their rubbers are indispensable.
1,4-цис полибутадиен, каучук, термодеструкция, кинетика, воздух, аргон, углекислый газ, 11,4-cis polyisoprene, rubber, thermal degradation, air, argon, carbonic gas
1. Madorskiy, S. Termicheskoe razlozhenie organicheskih polimerov, Moskva, Mir, 1967, 328 s.
2. D.V. Brazer, N.V. Shvarc, J. Appl. Polym. Sci. 22, 1, 113-124 (1987).
3. I. Ericsson, J. Chrom. Sci., 16, 8, 340-344 (1978)
4. H. Nakagawa, S. Tsuge, K. Murakami, J. Anal. Appl. Pyr., 10, 1. 31-40 (1986)
5. O.A. Korobeynikova, T.B. Minigaliev, V.P. Dorozhkin, Vestnik KGTU, 14, 11, 195-201 (2011).
6. 6. T.B. Minigaliev, O.A. Korobeynikova, V.P. Dorozhkin, Vestnik KGTU, 15, 18, 144-146 (2012).