In the present investigation is shown dielectric properties and molecular mobility urethane copolymers of 3,3-bis(azidomethyl) oxetane and 3-azidomethyl-3methyloxetane with various structures, such as B (AB) n, (BB) n, and (AB) n, where A - "soft blocks AMMO, B-" hard "blocks BAMO. The comparison of the results obtained earlier study by dielectric relaxation spectroscopy and thermal analysis and X-ray diffraction to identify the relaxation behavior of the structure.
диэлектрическая спектроскопия, 3, 3-биз(азидометил)оксетан, 3-азидометил-3метилоксетан, молекулярная подвижность, dielectric spectroscopy, 3, 3-biz (azidomethyl) oxetane, 3-аzidomethyl-3methyloxetane, molecular mobility
1. Yu.M. Mihaylov, E.R. Badamshina Energonasyschennye polimery: sintez, struktura, svoystva. M.: GosNIP «Raschet», 2008.
2. L.V. Karabanova, L.M. Sergeeva, A.V. Svyatyna, G. Seytre, G. Boiteux, I. Stevenson, Polimernyy zhurnal, 29, 4, 286-296 (2007).
3. T.N. Ishakov, N.A. Makarova, V.A. Petrov, N.V. Aver'yanova, M.R. Gibadullin, Vestnik kazanskogo tehnologicheskogo universiteta, 16,12 - 16 (2012).
4. V.A. Petrov N.V. Kuznecova, D.V. Pleshakov, Vestnik kazanskogo tehnologicheskogo universiteta,15, 332 (2011).
5. F. Kremer Broadband Dielectric Spectroscopy. Berlin, 2003. - 729c.