Distinction of ozonolize products of ethylene-propylene-diene rubbers with ethyleden-norbornene and dicyclopentadiene as the third somonomer is shown. Gluing ability of solutions of ozonized SKEPT is checked. The dynamic mechanical analysis of the initial, ozonized rubbers and rubber ozonized and subjected to heat treatment is carried out.
озонолиз, этиленпропилендиеновый каучук, этилиденнорборнен, дициклопентадиен, ozonolize, ethylene-propylene-diene rubber, ethylidene-norbornene, dicyclopentadiene